POPULATION INVERSION IN OPTICALY EXCITED ZnO CRYSTALS

T. Gulbinas1, M. Karaliūnas1

1 Semiconductor Physics Department and Institute of Applied Research, Vilnius University

Wide-band-gap semiconductors have attracted a great deal of attention because of ever-increasing commercial desire for light emitting devices in blue-UV spectral region. ZnO is one of these wide-band-gap ($E_g$ = 3.37 eV) semiconductors with characteristics promising for UV optoelectronics. One exceptionally interesting feature of ZnO is a huge exciton binding energy (60 meV) which makes possible existence of excitons and emission mechanisms involving these quasiparticles even at room temperature and above. Many of light-emitting devices operate under extreme conditions, in particular, at high pumping levels, which determine a variety of different optical transitions involving excitons especially at the threshold of population inversion. However, due to complexity of the processes many mechanisms still are far from understanding.

Here we present results of population inversion and optical gain (OG) experimental measurements in high-quality ZnO epitaxial films, growth on sapphire substrates with GaN buffer layers using molecular beam epitaxy. All measurements are performed at room temperature. The aim of this work is to analyze conditions of population inversion in ZnO, in particular, to determine the lasing threshold for excitation power density, as well as analysis of radiative transition mechanisms.

Photoluminescence (PL) and optical gain spectra have been analyzed over a wide range of excitation intensities using laser radiation with photon energy 3.49 eV and 4.66 eV. Stimulated emission peak was observed at $E_{ph}$= 3.175 eV. The PL analysis shows that mechanisms of stimulated emission involve exciton recombination. In particular interaction of excitons among themselves and with optical phonons is discussed. Measurements also show strong photon re-emission in ZnO epitaxial layers. This phenomenon was observed when underneath GaN buffer layer was exited and its emission lines could be resolved in PL spectra. Investigation of the PL dependence on excitation indicates that the threshold pumping power density is around ~700 kW/cm2, exceeding of which optical gain was observed.

OG coefficient was measured using so-called thin stripe technique (Shaklee method). Measurements with variable stripe length indicated maximum OG coefficient value of 190 cm-1. OG measurements by comparing two spectra for two different stripe lengths indicate blueshift of the gain maximum position when excitation increases. The reasons of OG dynamics in ZnO are discussed.