The influence of the electric field on the emission properties of the Sc-Ba dispensed emitters with the W matrix is studied in a high vacuum. In this work is shown, that in contrast with previous results [1], the increasing of electric field intensity, applied to emitter with W matrix at constant temperature, don't cause to substantial alteration chemical composition of emission-active matter.
The researches were carried out in UHV chamber and the pressure of residual gases did not exceed $5 \times 10^{-9}$ torr. The measurement of the emission properties was made in a flat diode system at a pulse mode. Pulse duration of the anodic voltage is 7 μs. The amplitude of anodic voltage can change up to 600 V. The anode was the molybdenum plate (2x2x0.2 sm.), which was heating to the high temperature by the electron impact. The emitter-anode spacing interval $d$ was equal to 1,2 mm, 1 mm, 0,8 mm and 0,6 mm and has been carefully controlled. Such set of distances allowed us to study influence of the electric field on the emissions properties of samples in the wide interval of field intensity.

For detailed analysis of the influence of electric field on the emission properties of Sc-Ba dispensed emitters with the W matrix and for comparison with the previous results for the emitters with Re-W matrix [1], it was made numerical calculation of the energy of displacement position of the maximum of electrons concentration in the emitters depends on electric field intensity for the case of a triangular potential barrier with the absence of image forces. The comparative analysis between experimental results and obtained calculated dependencies was made. Results of such comparison are shown on figure.
Obtained results shows, that presence and absence of qualitative agreement between numerically calculated dependencies and experimental data can be presented as one more argument that processes of forming of emitter's work surface with different material of matrices are substantial different.
As one can see from figure, with the increase of the electric field intensity for the sample with W matrix at constant temperature clear tendency for growing of slope of its voltage-current characteristic is presents. The only exception is characteristic, measured at the 1100 K. Such temperature is not sufficient to optimize chemical composition and microstructure of the emitter's surface.
The increasing of the electric field intensity, applied to emitters with W matrix at constant temperature don't cause to substantial alteration chemical composition of emission-active matter. Thus in the case of emitters with the W matrix the main factor of field emission is geometrical dimensions of crystallites and geometrical coefficient of the field amplification.