XP AND IMPEDANCE SPECTROSCOPY OF Li1,4Ti1,9P3O12 SOLID ELECTROLYTE CERAMICS

J. Banytė1, V. Venckutė1

1 Faculty of Physics of Vilnius University, Sauletekio ave. 9-III, LT-10222 Vilnius, Lithuania

The development of fast lithium conductors is attracting much of attention because of their applications in high-energy Li-ion batteries and electrochemical sensors [1, 2]. It is known that LiTi2P3O12 compound with the NASICON-type structure is a pure ionic conductor and its bulk ionic conductivity at room temperature was found to be $\sigma$ = 2⋅10-4 S/m [3]. High ionic conductivity of above mentioned NASICON- type structure solid electrolyte compounds stimulate further investigation of the materials. In the present work we report the technological conditions for the synthesis of LiTi2P3O12 powder, sintering of the ceramics, the results of the investigations of X-ray diffraction (XRD) from the powder, X-ray photoelectron spectroscopy (XPS) and electrical properties of the ceramics in the frequency range from 10 to 3⋅109 Hz in the temperature range from 300 to 600 K. The solid electrolyte compound was synthesized by a solid state reaction. The results of XRD have shown that at room temperature investigated compounds belong to hexagonal symmetry (space group $R$ 3c) with six formula units in the unit cell. Ti 2p, P 2p, O 1s and Li 1s core level XP spectra were fitted. It was ascertained that there are four different kinds of oxygen on the ceramic surface, including lattice oxygen, chemisorbed oxygen in the forms O2-, O22- and oxygen in hydroxyl environment (OH-). The deconvolution of the P2p core level XPS can be associated with different amounts of P5+ and P3+ states in the investigated ceramics. Two dispersion regions were found in conductivity spectra for investigated samples. The high frequency part of the recorded spectra may be attributed to the relaxation processes in grains, while the lower frequency part corresponds to relaxation processes in grain-boundary. The processes are thermally activated and dispersion regions shift toward higher frequencies as temperature increases. A good agreement is found between the activation energy of the ionic migration process in the grain and the activation energy of the characteristic relaxation frequency. It is shown that the major role in the temperature dependence of bulk conductivity is played by the Li+ ion mobility that increases as temperature increases.


[1] V. Thangadurai, J. Schwenzel, and W. Weppner, Ionics 11, 11 (2005).

[2] F. Salam, P. Birke, and W. Weppner, Electrochem. Solid-State Lett. 2, 201 (1999).

[3] H. Aono, E. Sugimoto, Y. Sadaoka, N. Imanoka, and G. Adachi, J. Electrochem. Soc. 137, 1023 (1990).