Dependence of the device electrical characteristics on fluence is essential in evaluation of the functionality of high-energy particle detectors under high fluence irradiation conditions. Irradiation by high energy particles is commonly applied to improve a switching speed of the semiconductor power devices. However, this enhancement of the switching speed can be achieved as a trade-off in optimizing the device characteristics when simultaneous degradation of static characteristics appears. In order to suppress the emerged radiation defects created during irradiation, the annealing technologies are routinely employed [1].
In this study, to control an impact of irradiation and anneal procedures, the voltage-current (I-V) characteristics were measured using Keithley 6430 electro-meter combined with internal 0-200V voltage source. Also, voltage-capacitance (C-V) characteristics were examined by using QuadTech 7600 LCR meter. In the latter case, a small ac test signal ($U_{ac}$≤20mV) regime has been applied, when the test signal is superimposed over a dc bias to measure the barrier capacitance. Capacitance characteristics were measured using $C_p$ and $C_s$ mode within 1kHz-1MHz frequency range, because C-V characteristics are crucially dependent on test signal frequency after heavy irradiations. In this study, the Si pad-detectors and power switches have been examined.
The CERN standard MCZ (Magnetic Czochralski) Si pad-detectors, irradiated by penetrative reactor neutrons with fluences ranging from 1012-1016 cm-2 and FZ (float zone) Si detectors, made at Hamamatsu company and irradiated with penetrative high-energy protons of fluences 1013 cm-2, were investigated. Additionally, to compare an impact of homogeneous and local damage by irradiations, the CZ (Czochralski) Si industrial power switches made at "Vilniaus Ventos Puslaidininkiai" company have been examined. The proton irradiations were performed by using a tandem accelerator at Helsinki University. The inhomogeneous δ-shape profile of radiation defects within stopping range of 2.0-2.3 MeV protons was formed in Cz Si using different fluences of 7·1012-1014 cm-2. The triangle profile of density of radiation defects was created by changing gradually an energy of protons in the range of 2-2.7 MeV and by properly varying irradiation fluence. Several irradiated samples were annealed at 120° C and 250°C temperature for 15 hours.
It has been obtained the linear increase of the leakage current with enhancement of fluence in the range of low and moderate irradiations. This increase of leakage current is caused by the radiation induced defects those act as the recombination and generation centres. However, the I-V characteristics become symmetrical, when comparing forward and reverse I-V branches, under irradiation with very large fluences. These observations can be explained by crucial reduction of carrier diffusion length and injection efficiency as well as by increase of leakage current. Analysis of the measured C-V characteristics also showed that high density of carrier traps are formed in FZ and MCZ Si pad-detectors. It was revealed that I-V characteristics of power switches depend on the damage profile and its location within the base region. The C-V characteristics enabled us to establish distribution of the effective charge density in the base region [2]. It has been revealed that heat treatments lead to transformation of radiation defects, however, suppression of radiation induced changes of leakage current and of barrier capacitance was not achieved for the range of applied anneal procedures.