SYNTHESIS AND LUMINESCENT PROPERTIES OF DOUBLE MIXED SCHEELITE-LIKE CALCIUM MOLYBDATE-TUNGSTATE COMPOUND

Gytautas Janulevičus1, Artūras Žalga1

1 Department of Applied Chemistry, Faculty of Chemistry, Vilnius University, Naugarduko Str. 24, 03225 Vilnius, Lithuania

In recent years, the tunable micro- and nano-structures with uniform shape and narrow size distribution have been of great interest in various researches and application fields. The synthesis of inorganic materials with varied morphology and texture, controlled crystallography, and micro- or nano-scale architectures is an important goal because of their novel chemical and physical properties. As one of important materials in the electro-optical industry, CaWO4 with scheelite-type structure has been of practical interest for a long time because of its attractive application in X-ray phosphors, scintillators, laser crystal, and host lattices in electron spin resonance. Moreover, many RE3+-doped scheelite related phosphors have also been studied extensively and reveal a non-radiative mechanism for energy transfer to the activator ion [1].

Energy transfer plays a crucial role in luminescent materials and the luminescence intensities are also various with the co-doped ions due to the existence of the energy transfer [2]. One of the potential high quantum yield red phosphors is Eu3+ incorporated CaMoO4 which belongs to scheelite related structure. The central Mo6+ ion is coordinated to four oxygen atoms in tetrahedral symmetry (Td). Hence molybdates are chemically stable and they can be a good choice for phosphors matrix.

Previous investigations have shown that the luminescent properties of CaMoO4:Eu3+ exhibited a desirable absorption in near-ultraviolet (UV) as well as a strong red emission. Therefore, these red phosphors can be potentially applied in LEDs for generating white light, and they have drawn considerable attention. By now, the improved luminescence is achieved via different methods, i. e. energy transfer from Bi3+, charge compensation by Li+, Na+, K+ and surfactants [3].

Synthesis process on the study of the crystal structure, surface morphology and luminescent properties of CaMo0.5W0.5O4:Na+, Eu3+ has not yet been reported, since most of CaMoO4:RE3+ and CaWO4:RE3+ phosphors were prepared by traditional solid state reaction. Zhou et al. reported the citric acid based sol-gel method which was used for the synthesis of CaMoO4:Eu3+ [4]. However, details on morphology of the particles were insufficient, and the influence of the complexing agent in the aqueous sol-gel synthesis on the crystallinity, morphology and optical properties is not clear. In the present work, the aqueous sol-gel method is applied to synthesize the Ca0.8Eu0.1Na0.1Mo0.5W0.5O4 particles . The crystal structure, surface morphology and luminescence of the as-prepared phosphors were also investigated in detail.


[1] F.Yu, J. Zuo, Z. Zhao et al., Low temperature synthesis and photoluminescent properties of CaMoO4:Eu3+ red phosphor with uniform micro-assemblies, Materials Research Bulletin 46, 1327-1332 (2011).

[2] Y. Jin, J. Zhang, Z. Hao et al., Synthesis and luminescence properties of clew-like CaMoO4:Sm3+, Eu3+, Journal of Alloys and Compounds 509, L348-L351 (2011).

[3] H. Wu, Y. Hu, W. Zhang et al., Sol-gel synthesis of Eu3+ incorporated CaMoO4: the enhanced luminescence performance, Journal of Sol-Gel Science Technology 62, 227-233 (2012).

[4] L. Zhou, L. Wang, F. Gong et al., Synthesis and photoluminescence of CaMoO4 superfine powder, Nature Science 32, 394-397.