Last decades laser assisted methods based on laser ablation and post-ablation irradiation in liquids has become a topic of great interest for targeted synthesis and modification of nanomaterials [1]. In the frame of the laser ablation technique one can combine particle synthesis with functionalization, encapsulation and stabilization of products. Post-ablation irradiation of nanoparticles with laser light can provide an effective way to alter their size and shape as well as to change a composition and inner structure of the particles. However, a practical application of laser methods for fabrication of nanoparticles with desired parameters requires a detailed study of physical processes (heating, melting, evaporation, laser-induced photofragmentation and aggregation) and chemical reactions accompanying laser-target and laser-particle interactions. The changes in nanoparticles induced by laser irradiation are determined by the temperature that is reached during the irradiation. Generally, on the first stage the incident radiation is absorbed by the particle that results in the temperature rise up to melting or even boiling point of the particle material. Exact knowledge of the particle temperature during pulsed laser irradiation is important for correct interpretation of the observed phenomena.
In the present work the capabilities of laser ablation technique with post-ablation irradiation in liquid for synthesis of doped zinc oxide nanoparticles and compound gadolinium-germano-silicides nanostructures has been studied. For controlling the temperature of the laser heated particles the emitted blackbody-like radiation from the hot nanoparticles have been measured and analyzed. Nanoscale compounds and alloys of gadolinium are promising materials for applications as magnetic agents for the hyperthermia treatment. ZnO nanostructures have received a great interest due potential applications in blue/UV light emitting diodes, piezoelectric transducers, gas sensors, etc., that require ZnO homojunctions formed at the interface between p- and n-type ZnO. Because of the intrinsic n-type conductivity, reliable p-type doping of ZnO is still a major problem although examples of p-type ZnO realization using acceptor dopants such as N, As or P, co-doping with nitrogen and a group-III element (Al, In) and dual-acceptor doping method with simultaneous introduction of two acceptors such as Li–N, N–As and N–Ag have been proposed.
The initial colloids were produced by laser ablation in ethanol or water solutions. The experiments were carried out by focusing of radiation of a Nd:YAG laser (LOTIS TII, LS2134D), operating in a double-pulse mode at 1064 nm, on the surface of the target placed in the cell with the solvent (repetition rate 10 Hz, pulse duration 8 ns, pulse energy 50 – 80 mJ). After the preparation the colloids were subjected to laser irradiation by the second harmonic of the Nd: YAG laser (wavelength 532 nm, pulse duration 10 ns) with fluences of 230 and 400 mJ/cm2. To prepare p-type ZnO NPs two different synthetic schemes were used. First, the ZnO doped NPs were synthesized by two step process which involved a sequential ablation of Zn and Ag targets in the 0.01 M NH4NO3 solution followed by the additional laser irradiation of the formed colloid with the second harmonic of the Nd:YAG laser (532 nm, 400 mJ/cm2) (ZnO N2). Second, the colloidal solution was obtained by laser ablation of Zn target in the mixture of Ag colloid in ethanol and NH4NO3. (ZnO N3). The compound Gd (Si, Ge) nanoparticles nanoparticles were synthesized by four step process which involved a sequential ablation of germanium, silicon and gadolinium targets followed by the additional laser irradiation of the mixture of the formed colloids.
The resulting NPs were characterized by TEM, XRD, SAED and optical absorption spectroscopy. To determine the temperature of the nanoparticles their thermal radiation spectra were fitted by a Planck curve, taking into account the emissivity function of nanoparticles and that the CCD detector counts the number of photons.
It has been shown that laser ablation of Zn target in $0.01~M~NH_4NO_3$ solution (N1) results in the formation of two types of particles: rod-like and spherical with a size of 30-50 nm. However, the phase composition of both types of particles is analogous. The major phase is polycrystalline ZnO with the hexagonal zincite structure. The impurity hexagonal zinc phase is also present in the diffraction patterns of both types of NPs. The ablation of Ag target in the solution N1 results in the transformation of rod-like particles into spherical ones (N2). The analysis of SAED patterns of the N3 sample showed that the particles are composed of the ZnO NPs in zincite structure and of cubic Ag. Laser irradiation of NPs in the third sample results in the disappearing of ZnO and Ag reflections that can be the consequence of the alloying of Ag and Zn NPs.
Laser assisted technique in liquid has been also demonstrated to be an effective tool to prepare magnetic Gd silicides and germano-silicides particles with sizes in the nanometric range. Magnetic measurements showed that the resulting nanoparticles didn't exhibit hysteresis at low temperature (6 K), which is typical to nanosized magnetic materials demonstrating superparamagnetic behavior.
It has been shown that the detection of black body radiation is a versatile tool for fast non-contact measurements of particle temperature. Based on the thermal radiation of the hot nanoparticles the temperature of the laser heated particles was determined. The resulting temperature (about 3000 K) was shown to be described on the basis of a balance between the absorbed laser energy and heat losses during the laser pulse using the bulk physical constants.