Femtosecond lasers provide us the ability to process materials with great precision. Because of the short pulse duration we can get smoother and cleaner side walls compared to picosecond and nanosecond lasers [1]. These advantages can be used for laser processing in semiconductor technology particularly for the fabrication of mask for ohmic contacts.
Molybdenum is used in semiconductor technology for its high melting point and one of the lowest coefficients of thermal expansion among commercially used metals. These qualities lead Mo to be the best choice for this particular technology. [2]

We present experimental results on micro-fabricated figures in a Molybdenum foil using 280 fs pulse high repetition rate Yb:KGW laser (central wavelength 1030 nm). The aspheric lens (F=4.03 mm and NA=0.62) was used to focus the laser beam on the molybdenum foil surface. The beam diameter on the surface of the foil was 1.7 μm. The optimal micro-fabrication parameters (the speed of the cutting, pulse energy and repetition rate) were evaluated for cutting of square and circle figures in 30 μm thickness Molybdenum foil. The squares and circles with sub-10×10 μm size were fabricated.