SPATIALLY RESOLVED LUMINESCENCE IN LGSO:CE CRYSTALS

M. Mackoit1

1 Semiconductor Physics Department and Institute of Applied Research, Vilnius University, Sauletekio al. 9 III, Vilnius, LT-10222, Lithuania

Oxide single crystals based on rare-earth silicates are known scintillators used in devices of medical diagnostics, scientific experiments on high-energy physics, particle physics and other applications. Mixed oxyorthosilicate crystals have been obtained in the last two decades. The enhancement of light yield in mixed crystals is a key issue for a range of applications. The improvement of light yield in LGSO:Ce might be produced by formation of Lu- and Gd-enriched regions. This short-range inhomogeneity might lead to formation of potential barriers limiting diffusion of thermalized uncorrelated carriers.

Confocal microscopy was used to study the spatial distribution of luminescence characteristics in LGSO:Ce crystals. CW laser diode (${\lambda}$ = 405 nm) was used for excitation. The objective with numerical aperture NA = 0.55 ensured the lateral resolution of 400 nm and axial resolution of 1600 nm.

The spatial distributions of luminescence parameters are strongly influenced by surface morphology. Deeper in the crystal, the LGSO:Ce and LSO:Ce luminescence spectra consist of one broad band peaked at ~510 nm. In LSO:Ce crystals, luminescence band position gradually shifts to longer wavelength with increasing distance from the surface. A detailed analysis of the spectra shows that the shift is accompanied by a decrease in intensity of the spectral component peaked at ~470 nm. Meanwhile, in LGSO:Ce crystals, spatial inhomogeneities (~1 to 3 μm in diameter) are observed in the band position images. Comparison of the spectra from areas with different band position reveals a strong variation in intensity at ~470 nm. Also, another spectral component peaked at ~600 nm was observed to have a strongly inhomogeneous spatial distribution.

The results show that the luminescence spectrum of LGSO:Ce consists of subbands, which are associated with CeO7 and CeO6 polyhedra. The intensity ratio of these subbands depends on activator distribution between these polyhedra, which, in turn, is influenced by Lu/Gd ratio in the crystal. With addition of Gd3+ with bigger ionic radius, the quantity of Ce3+ in six fold polyhedra increases due to loosening of crystal lattice. Therefore, it can be assumed that the spatial inhomogeneity of the spectral component (>550 nm) of LGSO:Ce reflect fluctuations in Lu/Gd ratio across the crystal.