The nanoscale morphology of bulk heterojunction solar devices has a great impact on the performance [1]. Weight ratio between donor:acceptor (D:A) and between acceptors ([60]PCBM and [70]PCBM), mixing non-halogenated solvents and thermal annealing were tested in Poly[[2,3-bis(3-octyloxyphenyl)-5,8-quinoxalinediyl]-2,5-thiophenediyl] (TQ1), [60]PCBM and [70]PCBM solar devices, with ITO/PEDOT:PSS/active layer/LiF/Al structure. Active layer was spin-coated from solution (20 mg/ml, solvent-o-xylene (except solvent testing part)). Photovoltaic characteristics were obtained by illumination with white light from solar spectrum simulator (AM1.5G). Morphology evaluation was done from Atomic Force Microscope (AFM) images and from Photoluminescence (PL) signal (425 nm exciting wavelength).
Devices with D:A ratio 1:2 (and 4:1 ratio of [60]:[70] PCBMs) had larger average short circuit current density ($J_{SC}=5.12 \text{ mA/cm}^2$), the average fill factor (FF=0.54) and the average power conversion efficiency (PCE=2.51 %) than 1:1 devices (4.30 mA/cm2, 0.52 and 2.07 %). PL and AFM data implied 1:1 (Fig. 1a) samples having fewer pure material domains, but too homogenous morphology might have led to poorer percolation of materials and less efficient charge transport than in 1:2 (Fig. 1b) blend.
1:0, 4:1, 1:1, 1:4 and 0:1 weight combinations of [60]PCBM:[70]PCBM were tested, keeping 1:2 (D:A). Nanoclusters grew bigger with the increase of the [70]PCBM amount (Fig 1c, d) leading to phase separation abd thus decrease of D:A interface area followed by loss of $J_{SC}$, FF and PCE (2.80 mA/cm2, 0.48 and 1.18 % in devices without [60]PCBM). The possible reason is worse sollubility of [70]PCBM than of [60]PCBM in o-xylene. Despite 1:0 blend having largest $J_{SC}$, FF and PCE, the ratio 4:1 was chosen for further improvement because of its thermal stability [2], which is important for printing process.
The small amount of additives with different vapour pressure than the main solvent may improve sollubility of fulerenes [3], so TQ1:[60]PCBM:[70]PCBM with the weight ratio 5:8:2 were dissolved in o-xylene:toluene with the following proportions: 1:0, 10:1, 1:1, 1:10 and 0:1. Toluene favoured demixing of the materials into separate phases (Fig. 1e, f), $J_{SC}$, FF and PCE were reduced with increasing toluene concentration in the blend.
In the last part devices were heated at 80 °C, 100 °C, 120 °C, 140 °C and 160 °C temperatures for 10 minutes before deposition of the electrodes. Heating promotes reorganization of materials into separate phases. The open-circuit voltage decreased with heating and stabilized at 120 °C (0.9 V at room temperature and 0.8 V at 120-160 °C). Annealing reduced $J_{SC}$ as well, leaving not annealed samples with the best perfomance. The morphology probably was already optimal under the chosen preparation conditions; annealing possibly would have improved performance of 1:1 (D:A) blend [2], which had less demixed phase and thus more complicated paths for charge transport than 1:2 blend.