In the past decades, fast oxygen-ion conductors attracted considerable attention of many scientists due to their unique properties and many relevant applications in solid oxide fuel cells, oxygen sensors and oxygen pumping devices [1]. One of the main requirements for such devices is to obtain high ionic conductivity. Nowadays, the most popular materials used as solid electrolytes are yttria-stabilized zirconia (YSZ), scandia stabilized zirconia (ScSZ) and gadolinium doped ceria (GDC). However, these electrolytes works at high temperatures (operating temperature 1,073 – 1,273 K) and limits the commercialization. Laccore et al. reported a promising LAMOX family materials, which exhibits high oxide-ion conductivity at intermediate operating temperature (873 – 973 K). Unfortunately, La2Mo2O9 has some disadvantages, poor ionic conductivity at low temperatures and degradation in reducing environments [2].
La2Mo2O9 exists in two crystalline forms: monoclinic α phase (P21) that occurs at room temperature with a very low conductivity and cubic β phase (P213), which is stabile above 853 K [3]. After phase transition the oxide-ion conductivity increases sharply reaching values higher than those of YSZ (0,06 S/m at 800°C) [4]. In order to stabilize β-phase of the lanthanum molybdate in low temperature and decrease the degradation in reducing environments, K+, Sr2+, Ba2+,Ca2+, Bi3+, V5+, S6+, Cr6+, W6+, and other ions can be used to suppress the phase transition to the α-phase.
In this paper, we report the environment friendly synthesis method to synthesize La2-xDyxMo2O9. All La–Dy–Mo–O tartrate gel precursors for La2-xDyxMo2O9 ceramics (x=0.005, 0.01, 0.025, 0.05, 0.1, 0.2) were prepared by an aqueous sol-gel technique in the sol-gel process using tartaric acid as a ligand. The obtained La–Dy–Mo–O tartrate gels were dried at 393 K and heat treated at 473 K, 673 K, 873 K, 1,073 K, 1,273 K and 1,473 K of temperatures, respectively. Raman spectroscopy and X-Ray diffraction were applied for the detailed investigation of the phase transition from the metastabile high-temperature cubic α-phase to the room-temperature α-crystalline modification. In addition, the suppression of the phase transition by addition of the dysprosium amount according to the vibrational, rotational, and other low-frequency modes in the La2Mo2O9 was also studied.