During the last decade solid oxide fuel cells (SOFC's) have been intensely investigated as a next generation green energy system because they exhibit high ionic conductivity, chemical and thermal stability and also have high efficiency and generate low pollution emissions [1]. Recent SOFC's has been focused on the development of intermediate and low operating temperature range of 300-800 °C considering long-term performance stability, high conversion efficiency, and low equipment material cost [2].
The most widely used ceramic in SOFC is yttria stabilized zirconium (YSZ) ceramic. It is a traditional fuel cell electrolyte and must typically be operated at high temperatures, due to its relatively high ionic resistivity at lower temperatures. Also this ceramic presents the metastable tetragonal phase which is essential for the structural hardening during cooling. Meanwhile, gadolinia-doped ceria (GDC, $Ce_{0.9}Gd_{0.1}O_{1.95}$) is considered to be one of the most promising electrolytes for SOFCs to be operated below 650 °C [3]. Owing to high oxygen-ionic conductivity and good chemical compatibility, Gd-doped CeO2-based ceramics are popularly an upcoming alternative to yttria-stabilized zirconia (YSZ) as solid electrolyte in intermediate and low temperature SOFC applications [4]. To address the significant problem with ceria based materials a number of approaches have been taken, such as finding the ideal doping level and ion to balance stability with adequate oxide ion conductivity, decreasing the operating temperature and improving materials processing etc [5].
The implement of these challenges could be successfully reached by using so-called solution-based synthetic methods, which play a crucial role in the design and production of fine ceramics, in addition, these methods have been successful in overcoming many limitations of the traditional solid-state, high-temperature methods.
In this study we report the aqueous sol-gel synthesis technique for the preparation of YSZ and GDC ceramics, which were additionally annealed at 700, 800, 900, 1,000, 1,100 and 1,200 °C temperatures. Moreover, in order to proof a difference between separate solid electrolytes the thermal decomposition of the as-prepared gels and the crystal phase stability according to the sintering temperature of the double oxides by thermogravimetric analysis, differential scanning calorimetry (TG–DTA) and X–Ray diffraction (XRD) measurements were additionally investigated. Besides, the research of the surface morphology and the characteristic vibrations of the functional groups by scanning electron microscopy (SEM) and Fourier transform infrared spectroscopy (FT–IR) were also performed.