In the last years a large interest to investigations of various nanosized objects has been developed in concern with their exhibition of interesting characteristic properties, being indistinctive for materials with macro- and microscopic properties. The most simple and logical method of a creation of nanomaterials is the use of nanoporous matrices (templates), as natural conditions of self-organization of nanosized objects are realized in the pores. Using of the pores makes it possible to obtain nanoparticles and nanofibres of semiconductors [1], metals [2], multilayers of metals [3], etc. Some structures of this kind possess a sensitivity to light, humidity, organic substances, and could be used as sensors [4]. Depending on the nature of the material placed in pores, the obtained nanostructures could be used for a construction of resistors, capacitors, diodes and inductors [5]. At present, porous Al2O3, TiO2, polycarbonate and polyimide membranes are used for a creation of nano-objects [6, 7]. Still, from the point of view of an implementation of nanosystems on the base of silicon in modern technological processes, most prospective are the use of templates on the base of silicon oxide. Pores in a-SiO2 layer can be obtained with the implementation of the swift heavy ion (SHI) track technology, which includes irradiation with the SHIs and chemical etching [8].
The process of chemical etching in solutions of hydrofluoric acid of swift heavy ion tracks in a-SiO2 depends on the energy of electronic loss (dE/dx)e and has a threshold character. At the (dE/dx)e value less than 1.5 keV · nm-1, pores formation is impossible. At the (dE/dx)e values in the range ~ 1.5 – 4 keV · nm-1 the etching process is possible, but obtained pores are characterized by various diameters and angles of the etching cone, as well as by a not high etching efficiency (not all the ion tracks are transformed into pores). The energy value of about 4 keV · nm-1 is a necessary condition for the obtaining of pores with a uniform distribution of forms and dimensions with the etching efficiency ~ 100 %. At the electronic loss energies of more than 4 keV · nm-1, the pore diameters depend on the (dE/dx)e value and their sizes increase with the rise of this loss at the same etching conditions [9].
We have given a proposition that at large energy loss energies (> 15 keV · nm-1) pore diameters will not depend on the (dE/dx)e value at the same etching conditions. This assumption could be justified on the base of the following arguments. The transfer of energy of the bombarding ion to the lattice by means of the equilibrium thermodynamic processes takes place in nanoscopic scales during particularly short period of time. Since the temperature equilibrium is achieved after the ten atomic collisions during the time period 10-13 s, the local temperature equilibrium at such a high temperatures and short time scales can take place only in the limit of 0.5 nm. As the energy can propagate on small distances, first a melting and evaporation of material inside the ion track, and only then its diameter will increase. It should be noted that an absence of the dependence of the pore diameter on the electron energy loss at (dE/dx)e > 15 keV/nm has been noted as well in the work [9].
A systematic investigation of results of the ion track etching in the a-SiO2 layer, obtained at the irradiation by 132Xe, 152Sm, 197Au and 238U ions with (dE/dx)e values in the range from 16 to 23 keV · nm-1 has made it possible to introduce the new threshold value (dE/dx)e > 15 keV · nm-1. With that the pore diameters have a constant size independently on the value of electronic loss energy. Results of the present investigation make it possible to forecast obtaining of the a-SiO2-based porous templates with a pre-determined geometrical parameters, independently of the irradiating ion with a high precision.