For the past 40-50 years, lead base perovskite Pb(ZrxTi1-x)O3 (PZT) piezoelectric ceramics have dominated the commercial market of piezoelectric devices due to their remarkable dielectric and piezoelectric properties and ability to operate in wide temperature range [1].
BaTiO3 perhaps the most widely researched perovskite in the last decades. Inserting potassium niobate to BT structure creates stresses that increases domain wall count and in result piezoelectric coefficient [2] KNBT has comparable piezoelectric coefficient, thus making it a great substitute. The fact that KNBT is lead free ceramic makes it of high interest for both researchers and engineers due to environmental concerns.
KNBT composites were prepared in two steps: compact BT particles were heated to 1000°C for 2h to create low-density ceramics, then KN were epitaxially deposited to BT structure. [3]
In this presentation dielectric properties of KNBT with different KN molar ratios will be presented. From Figure 1 we can observe that the bigger the KN/BT ratio is, the more obscured phase transitions of BaTiO3 become. Low dielectric permittivities in KN/BT with molar ratios of 0.22 and 0.5 can be explained by its low relative density. At frequencies from 107 to 1011 Hz dipole relaxation can be observed with relative relaxation time about 60-70 ps (figure 2).