ZnGa₂O₄ SPINEL NANOPHOSPHORS WITH PERSISTENT LUMINESCENCE FOR BIOIMAGING

Vilius Čirgelis1, 2, Simona Streckaitė1, Vitalii Boiko3, Lena Golubewa1, Vidas Pakštas1, Mariusz Stefanski3, Dariusz Hreniak3, Vidmantas Gulbinas1

1 Center for Physical Sciences and Technology, Sauletekio Ave. 3, 10257 Vilnius, Lithuania

2 Vilnius University, Faculty of Physics, Sauletekio Ave. 9, 10222 Vilnius, Lithuania

3 Polish Academy of Sciences, Institute of Low Temperature and Structure Research, Okolna 2, 5-422 Wroclaw, Poland

Zinc gallium oxide (ZnGa\(_{2}\)O\(_{4}\), ZGO) is a cubic spinel-structured oxide that has attracted interest for applications in optoelectronics [1], plasmonics [2] and biomedicine [3]. ZGO is chemically stable, inert to oxygen and humidity, and biocompatible, making it promising phosphor for applications, like bio-imaging and theranostic [4]. In ZGO lattice, Zn2+ occupies tetrahedral sites and Ga3+ occupies octahedral sites. Since chemical synthesis is entropy driven process, partial cation inversion can occur, where a fraction of Zn2+ occupies octahedral and a fraction of Ga3+ occupies tetrahedral positions, forming antisite defects. Antisites introduce trap states that capture charge carriers and hinder their recombination, enabling long-lived energy storage of excitation energy on timescales from hours to days [5]. The delayed photon emission, occurring from exciton recombination is called persistent luminescence (PersL). PersL is advantageous for in vivo bioimaging because the material can be pre-charged ex vivo and subsequently injected into organism, allowing imaging without continious excitation, thereby reducing tissue autofluorescence and minimizing phototoxicity and thermal damage [6]. ZGO optical properties can be altered by introduction of rare-earth ions into the lattice. Emission from Cr³⁺ and Yb³⁺ overlaps with the first and second biological windows—spectral ranges where tissue absorption and scattering are relatively low—enabling efficient deep-tissue imaging.

In this study, Cr³⁺ doped ZnGa₂O₄ was synthesized hydrothermally from aqueous solutions of Zn(NO₃)₂, Ga(NO₃)₃, and Cr(NO₃)₃. Stoichiometric amounts of the metal-nitrate precursors were combined and the pH was adjusted to 8 using NH₄OH. The mixture was transferred to a Teflon-lined vessel and sealed in a stainless-steel autoclave for hydrothermal treatment at 200 °C for 24 h. The resulting powder was washed with water and ethanol, dried for 24 h, and annealed at temperatures between 200 °C and 900 °C for 3 hours. The structural and optical properties of ZGO:Cr³⁺ were characterized by X-ray diffraction (XRD), steady-state and time-resolved photoluminescence (PL), thermoluminescence, and diffuse reflectance spectroscopy.

XRD measurements confirm that the synthesized ZnGa₂O₄ materials crystallize in the cubic spinel structure. With increasing annealing temperature, the diffraction peaks become narrower, indicating improved crystallinity and crystallite growth (i.e., reduced microstrain/defect-related broadening) over the range from 0 to 800 °C. At 800 °C, the XRD pattern matches that of the pre-annealed sample, indicating phase transition. The highest steady-state PL intensity is observed for ZGO:Cr³⁺ with 1.00 mol% Cr³⁺, whereas the longest persistent-luminescence decay is obtained for the 0.25 mol% Cr³⁺-doped sample. As ongoing work, ZGO:Yb³⁺ samples will be characterized using the same set of techniques.

Acknowledgments: This research was funded by Polish-Lithuanian research project DAINA-3, agreement No [S-LL-24-11].


[1] Y.-C. Shen, C.-Y. Tung, C.-Y. Huang, Y.-C. Lin, Y.-G. Lin, and R.-H. Horng, “Study on Optoelectronic Characteristics of ZNGA2O4 Thin-Film Phototransistors,” ACS Applied Electronic Materials, vol. 1, no. 5, pp. 783–788, May 2019, doi: 10.1021/acsaelm.9b00128.

[2] M. Runowski et al., “Preparation of biocompatible, Luminescent-Plasmonic Core/Shell nanomaterials based on lanthanide and gold nanoparticles exhibiting SERS effects,” The Journal of Physical Chemistry C, vol. 120, no. 41, pp. 23788–23798, Sep. 2016, doi: 10.1021/acs.jpcc.6b06644.

[3] Z. Li et al., “In vivo repeatedly charging Near‐Infrared‐Emitting mesoporous SIO2/ZNGA2O4:CR3+ persistent luminescence nanocomposites,” Advanced Science, vol. 2, no. 3, Feb. 2015, doi: 10.1002/advs.201500001.

[4] D. Ding et al., “Mn3+-rich oxide/persistent luminescence nanoparticles achieve light-free generation of singlet oxygen and hydroxyl radicals for responsive imaging and tumor treatment,” Theranostics, vol. 11, no. 15, pp. 7439–7449, Jan. 2021, doi: 10.7150/thno.62437.

[5] T. Zhao, R. Abdurahman, R. Aiwaili, S. Wu, and X.-B. Yin, “Spinel-type persistent luminescence nanoparticles: From mechanisms, compositions to applications,” Coordination Chemistry Reviews, vol. 488, p. 215171, Apr. 2023, doi: 10.1016/j.ccr.2023.215171.

[6] S. Wu, Y. Li, W. Ding, L. Xu, Y. Ma, and L. Zhang, “Recent advances of persistent luminescence nanoparticles in bioapplications,” Nano-Micro Letters, vol. 12, no. 1, p. 70, Mar. 2020, doi: 10.1007/s40820-020-0404-8.