Bimetallic structures are an excellent solution for a lot of engineering applications which require varying properties at different locations of the same object. Implementation of such structures into engineering fields can lead to easier maintenance, economical and space savings and can also open wider application possibilities [1].
In recent years, production of bimetallic structures has been made possible with help of additive manufacturing (AM) technologies. Using laser powder-bed fusion AM, bimetallic structures can be created by depositing different materials in a layer-by layer fashion.
In this work, two materials in powder form were used for bimetallic structure formation – 17-4 PH stainless-steel and CoCr. According to SEM-EDS results, the two materials consist of 73.8 at. % Fe, 16.0 at. % Cr, 4.6 at. % Ni, 4.2 at. % Cu and 61.8 at. % Co, 29.4 at. % Cr, 6.9 at. % Mo accordingly. Particle size distribution is similar for both materials and is in the range of 10-80 μm.
The bimetallic structure (Fig. 1) was successfully produced by using the direct metal laser sintering (DMLS) technology applied in EOSINT M280 machine.

In-depth analysis of the 17-4 PH SS and CoCr materials and microstructural properties of the produced bimetallic sample were investigated and will be presented in this work.