ADDITIVE-FREE POLYMERIC TRIARYLAMINE DERIVATIVES AS HOLE TRANSPORTING MATERIALS FOR STABLE PEROVSKITE SOLAR CELLS

Taisuke Matsui1, Ieva Petrikyte2, Tadas Malinauskas2, Konrad Domanski3, Maryte Daskeviciene2, Matas Steponaitis2, Paul Gratia4, Wolfgang Tress3, Juan-Pablo Correa-Baena3, Antonio Abate3, Anders Hagfeldt3, Michael Graetzel3, Mohammad Khaja Nazeeruddin3, Vytautas Getautis2, Michael Saliba3, 4

1 Advanced Research Division, Materials Research Laboratory, Panasonic Corporation, 1006 Kadoma, Kadoma City, Osaka 571-8501, Japan

2 Department of Organic Chemistry, Kaunas University of Technology, Radvilenu pl. 19, Kaunas, 50254, Lithuania

3 Laboratory of Photonics and Interfaces, Institute of Chemical Sciences and Engineering, École Polytechnique Fédérale de Lausanne, Lausanne CH-1015, Switzerland

4 Group for Molecular Engineering of Functional Materials, Institute of Chemical Sciences and Engineering, École Polytechnique Fédérale de Lausanne, Lausanne CH-1015, Switzerland

5 Laboratory of Photomolecular Science, Station 6, CH-1015 Lausanne, Switzerland

Today organic optoelectronics require ability to create devices by solution deposition methods, preferably using simple, inexpensive and easily purified materials. Organic photovoltaic devices are made of multiple layers and high performance is only possible using materials which have good compatibility with each other. Some of those requirements include the stability issue, which derives from additives that are used in the process of increasing the conductivity of hole transporting materials.

Having that in mind triarylamine derivative polymers with different functional groups were synthetized as hole transport materials (HTMs) for perovskite solar cells (PSCs). The novel materials enabled efficient PSCs without the use of chemical doping to enhance the charge transport. Devices employing poly(triarylamine) with methylphenylethenyl functional groups showed better power conversion efficiency then widely used additive-free compound - poly[bis(4-phenyl)(2,4,6-trimethylphenyl)amine] (PTAA). Notably, devices with the foremost polymer enabled stable PSCs under 1 sun at maximum power point tracking for ~40 hours and under elevated temperature (85 °C) for more than 140 hours. The results present remarkable progress towards stable PSC under real working conditions, which is crucial for industrial application.